The bed height of resin is 1. 2 m and the volume is about 2. 7 m3. In order to regenerate the exhausted resin out of the bed, the predesigned condensate polishing mixed bed regeneration process was used to regenerate the first exhausted resin.
树脂层高1.2m,体积约2.7m~3。为了对失效后树脂进行体外再生,采用预定的凝结水净化混床再生工艺条件对首次失效的混床树脂进行了再生试验。